ThermalEast
// SPEC · 耐火砖

电熔镁砖 MgO 97%

MgO 97%电熔镁砖,以高纯电熔镁砂为原料,气孔率极低,抗渣渗透与抗高温蠕变性能卓越,使用温度达1900°C,适用于电弧炉热点区、AOD转炉渣线及RH精炼炉下部。

耐火砖最高温度: 1900°CGB/T 2275

// 主要特性

  • Electrofused MgO grain delivering highest achievable purity and density
  • Extremely low apparent porosity blocking slag and steel penetration
  • Outstanding creep resistance sustaining loads above 1800°C
  • Excellent corrosion resistance to both basic and neutral steelmaking slags

// 技术规格

CaO (%)≤0.8
MgO (%)≥97
Apparent Porosity (%)≤12
Cold Crushing Strength (MPa)≥65
Refractoriness Under Load (°C)≥1700

// 应用领域

EAF hotspot sidewall working liningEAF roof delta sectionAOD converter slag line liningRH degasser lower vessel working liningLadle hot-metal zone working lining
// 快速规格
最高温度1900°C
导热系数5.8 W/(m·K) at 1000°C
体积密度3.10 g/cm³
执行标准GB/T 2275