ThermalEast
// SPEC · 耐火砖

低碳镁碳砖 MgO 78% C 8%

MgO 78% C 8%低碳镁碳砖,碳含量低,有效降低钢液增碳风险,有利于洁净钢生产,抗渣腐蚀性强,适用于LF精炼钢包渣线、RH插入管及VOD等二次冶金设备。

耐火砖最高温度: 1750°CGB/T 20110

// 主要特性

  • Reduced carbon content minimizing steel recarburization risk
  • High MgO content delivering excellent slag corrosion resistance
  • Low apparent porosity improving resistance to slag infiltration
  • Suited for IF steel and ultra-low carbon grade clean steel production

// 技术规格

CaO (%)≤1.2
MgO (%)≥78
Apparent Porosity (%)≤4
Cold Crushing Strength (MPa)≥28
Refractoriness Under Load (°C)≥1680

// 应用领域

Ladle slag zone working liningLF ladle furnace working liningRH degasser snorkel liningVOD vessel lining for ultra-low carbon steel gradesSecondary metallurgy vessel working lining
// 快速规格
最高温度1750°C
导热系数5.5 W/(m·K) at 1000°C
体积密度3.03 g/cm³
执行标准GB/T 20110
// 获取报价

申请报价