// SPEC · 不定形耐火材料
碳化硅质耐火泥浆 SiC 50%
碳化硅含量50%的SiC耐火泥浆,导热性高,耐磨损和抗氧化性能优异,热膨胀与SiC砖体相匹配,适用于SiC窑具砌筑、陶瓷隧道窑碳化硅砖砌体及锌蒸馏炉SiC衬体的砖缝结合。
// 主要特性
- High thermal conductivity closely matching SiC brick and kiln furniture substrate
- Excellent abrasion and particle erosion resistance at elevated temperature
- Compatible thermal expansion coefficient with nitride-bonded and oxide-bonded SiC
- Good oxidation resistance in kiln and furnace oxidizing atmospheres
// 技术规格
| Al2O3 (%) | ≥20 |
| Consistency (mm) | 100–135 |
| Water Addition (%) | 18–23 |
| Bond Strength (MPa) | ≥3.5 |
| Max Service Temp (°C) | 1400 |
// 应用领域
SiC kiln furniture (batts, saggers, posts) joint bondingSilicon carbide brick masonry in ceramic and sanitaryware tunnel kilnsZinc smelting retort furnace SiC lining brick jointsNon-ferrous metal refining furnace SiC sidewall panelsWaste-to-energy boiler lower furnace SiC membrane wall panel joints
// 快速规格
最高温度1400°C
导热系数6.5 W/(m·K) at 600°C
体积密度2.40 g/cm³
执行标准GB/T 22459
// 获取报价