ThermalEast
// SPEC · 耐火砖

熔铸AZS-36耐火砖

AZS-36熔铸耐火砖,ZrO2含量36%,专为玻璃窑炉喉部及胸墙设计,高锆含量降低析晶相渗出风险,适用于浮法、电子玻璃及光学玻璃熔窑关键部位,耐侵蚀性优于AZS-33。

耐火砖最高温度: 1650°CYB/T 391

// 主要特性

  • Premium glass melt corrosion resistance exceeding AZS 33# grade
  • Ultra-low porosity (<1%) preventing glass inclusion defects
  • Reduced exudation phase minimizing downstream glass contamination
  • Enhanced structural integrity at glass furnace throat operating temperatures

// 技术规格

SiO2 (%)≤15.0
ZrO2 (%)≥36.0
Al2O3 (%)≥47.0
Apparent Porosity (%)≤1.0
Bulk Density (g/cm³)≥3.48

// 应用领域

Float glass furnace throat blockGlass furnace breast wall liningE-glass fiber furnace critical zone liningOptical glass melting furnace working liningLCD glass substrate furnace high-contact zones
// 快速规格
最高温度1650°C
导热系数2.7 W/(m·K) at 1000°C
体积密度3.50 g/cm³
执行标准YB/T 391
// 获取报价

申请报价