ThermalEast
// SPEC · 耐火砖

低蠕变粘土砖 Al2O3 43%

低蠕变粘土砖,Al2O3 43%,高温荷重变形率低,尺寸稳定性优,适用于窑车台面、炉拱及回转窑托圈,适合水泥和石灰回转窑。

耐火砖最高温度: 1430°CGB/T 2493

// 主要特性

  • Low creep rate at 1400°C for dimensional stability under sustained load
  • High refractoriness under load ≥1370°C for arch and roof applications
  • Uniform dense texture minimising stress concentration in arch structures
  • Extended campaign life under cyclic thermal loading conditions

// 技术规格

Al2O3 (%)≥43
Fe2O3 (%)≤1.8
Apparent Porosity (%)≤18
Cold Crushing Strength (MPa)≥45
Refractoriness Under Load (°C)≥1370

// 应用领域

Tunnel kiln car deckFurnace roof and arch structureRotary kiln riding ring bearing zoneShuttle kiln sidewall and crownLime shaft kiln shaft lining
// 快速规格
最高温度1430°C
导热系数1.15 W/(m·K) at 600°C
体积密度2.28 g/cm³
执行标准GB/T 2493
// 获取报价

申请报价