ThermalEast
// SPEC · 耐火砖

磷酸盐结合粘土砖 Al2O3 42%

磷酸盐结合粘土砖,Al2O3 42%,常温固化无需高温烧成,适用于焦炉热修、回转窑补砌及紧急炉衬维修,快速恢复生产。

耐火砖最高温度: 1420°CGB/T 2493

// 主要特性

  • Rapid cold-setting bond eliminates high-temperature kiln firing requirement
  • High initial green strength enabling fast repair turnaround
  • Good adhesion compatibility with existing fired refractory linings
  • Retained mechanical strength after repeated thermal cycling to 1420°C

// 技术规格

Al2O3 (%)≥42
Fe2O3 (%)≤2.0
Apparent Porosity (%)≤19
Cold Crushing Strength (MPa)≥55
Refractoriness Under Load (°C)≥1350

// 应用领域

Coke oven wall hot repairRotary kiln spot patching and reliningBlast furnace tuyere zone emergency repairSteel ladle preheating station lining patchReheat furnace skid pipe sleeve replacement
// 快速规格
最高温度1420°C
导热系数1.1 W/(m·K) at 600°C
体积密度2.32 g/cm³
执行标准GB/T 2493