// SPEC · Monolithic Refractories
Magnesia-Carbon Ramming Mix MgO 75% C 5%
Magnesia-carbon ramming mix MgO 75% + C 5% for EAF delta zone, tapping spout, and converter tap pad. High basic slag erosion resistance with excellent thermal shock performance in intensive steelmaking service.
// Key Features
- Carbon matrix bonding for outstanding thermal shock resistance
- High erosion resistance against FeO-rich basic steelmaking slag
- Rapid field sintering enabling fast furnace turnaround
- Self-sintering behavior at operating temperature reducing downtime
// Technical Specifications
| Cold CCS (MPa) | 40 |
| Grain Size (mm) | 0–5 |
| Main Component (%) | MgO ≥ 75, C ≥ 5 |
| Sintering Temp (°C) | 1300 |
| Max Service Temp (°C) | 1750 |
// Applications
EAF delta zone and sidewall hot-spot repairEAF tapping spout liningConverter tap pad and taphole surroundLadle slag line emergency patch repairElectric arc furnace bottom ramming layer
// Quick Specs
Max Temperature1750°C
Density2.88 g/cm³
StandardYB/T 5013
// Get Pricing
WhatsApp Us